Home Improvement

Red Clay Bricks: Types, Grades and Uses Around the Home

Red Clay Bricks: Types, Grades and Uses Around the Home

Two bricks can look identical in a pallet and still fail very differently once they are in the ground. Red clay bricks are fired from shale and clay, and the red color comes mostly from iron oxide in the clay. What separates a brick that lasts a century from one that crumbles after a few winters is its type and grade, not its color.

For most home projects, the short answer is this: use face brick for anything people will see, paving brick for patios and walks, and a severe weathering (SW) grade anywhere the brick touches soil or sits in a freeze-thaw climate. Common or building brick is fine for hidden backup walls, and a moderate weathering (MW) grade works in milder climates or protected spots.

The table and sections that follow explain each brick type, how US grades work, how clay compares with red concrete brick, and how to choose, cut and lay them safely.

Red Clay Bricks: Types at a Glance

Type What it is Typical home uses
Common (building) brick Basic structural brick with less focus on looks Backup walls, hidden structure, fill
Face brick Made for appearance, with tighter size and color control Veneer walls, chimneys, garden walls, planters
Paving brick (pavers) Dense, hard-fired brick made for foot or vehicle traffic Patios, walkways, driveways, edging
Solid brick No holes, or cores taking up no more than 25 percent of the bed area Paving, caps, exposed edges, steps
Cored brick Holes through the brick that cut weight and help mortar grip Most veneer walls
Hollow brick Larger cores, over 25 percent of the bed area Reinforced masonry walls
Engineering-style brick Very dense, low-absorption brick (a UK term) Damp courses, retaining walls, below grade
Firebrick Refractory brick for high heat, usually buff not red Fireplace and pizza oven linings

You will see “engineering brick” in a lot of online searches. It is a British classification for very dense, low-absorption brick. In the US, the closest equivalent is a high-strength, SW-grade face or paving brick with low absorption.

Understanding Brick Grades: SW, MW and NW

US building and face bricks are graded by how well they resist weathering, especially water soaking in and freezing.

  • SW (severe weathering): high resistance to freeze-thaw damage. Choose it for anything in contact with soil, on horizontal surfaces, or in cold climates with frequent freezing.
  • MW (moderate weathering): moderate resistance. Suits vertical walls above grade in milder climates where the brick is unlikely to be soaked and frozen.
  • NW (negligible weathering): for interior or fully protected uses only, and mainly seen in common brick.

Face brick also has appearance types. FBS is the standard type with normal size and color variation, FBX has tighter tolerances for a crisper, more uniform look, and FBA is intentionally irregular for an antique or handmade style. Paving bricks use their own classes based on traffic and weathering exposure. When in doubt, ask the supplier which grade and class the brick meets and confirm it suits your climate.

Clay vs Red Concrete Brick

Red concrete brick looks similar from a distance but is made from cement, sand and aggregate with pigment added. That difference shows up over time.

Factor Red clay brick Red concrete brick
Color From the clay itself, runs through the brick Pigment that can fade on the surface
Size changes Grows very slightly over time as it absorbs moisture Shrinks slightly as it cures and dries
Weight Somewhat lighter for the same size Somewhat heavier
Cost Usually higher Usually lower
Look Natural variation, classic finish More uniform, can look flatter

Because clay grows and concrete shrinks, do not mix the two in the same wall without expansion and control joints designed for both. For a patio, either works if it is rated for paving; clay holds its color longer, while concrete pavers are usually cheaper and easier to find in interlocking shapes.

Common Uses Around the Home

Patios and walkways

Use solid paving brick laid on a compacted gravel base and a sand setting bed, or set in mortar on a concrete slab. Standard building brick with cores should not be used flat on the ground because water fills the holes and freezes.

Garden walls and planters

Face brick in SW grade suits low garden walls, raised beds and mailbox columns. Cap the top with solid brick or stone that sheds water.

Veneer and accent walls

Cored face brick is standard for exterior veneer. Interior accent walls often use thin brick, which is real clay brick sliced to about half an inch thick.

Edging and borders

A row of solid brick on edge or a soldier course makes a durable lawn or bed border.

Tools and Materials

  • Brick chisel (also called a brick set) and a 3 to 4 pound hand sledge
  • Angle grinder or wet saw with a masonry blade
  • Mason’s trowel, pointing trowel and jointer
  • Line, line blocks and a 4-foot level
  • Type N or Type S mortar (Type S for below-grade or load-bearing jobs)
  • Compactable gravel, coarse sand and a plate compactor for paving
  • N95 or P100 respirator, safety glasses, hearing protection and gloves

A brick chisel is the cleanest way to split full bricks for a running bond. Score all four faces, then strike firmly on the face you want to keep.

Looking to buy Red Clay Bricks? Compare top-rated options.
Shop on Amazon →Browse Our Shop
As an Amazon Associate we earn from qualifying purchases.

How to Choose and Lay Brick for a Small Project

  1. Define the exposure. Note if the brick touches soil, lies flat, or faces hard freezes. Any of those calls for SW grade or a rated paver.
  2. Pick the type. Face brick for visible walls, paving brick for walking surfaces, common brick only where it will be hidden.
  3. Order extra. Add 5 to 10 percent for cuts and breakage, and buy from one production run so color matches.
  4. Prepare the base. For walls, pour a footing below the frost line per local code. For patios, excavate, then compact several inches of gravel in lifts.
  5. Check absorption. Sprinkle water on a brick. If it disappears in under a minute, wet the bricks lightly before laying so they do not pull water out of the mortar.
  6. Lay to a line. Set leads at each end, stretch a line and fill between them, checking level and plumb often.
  7. Tool the joints. When mortar is thumbprint hard, strike joints with a concave jointer to shed water.
  8. Clean carefully. Brush off crumbs and follow the brick maker’s guidance before using any masonry cleaner.

Dust Safety When Cutting Brick

Cutting, grinding or chiseling clay brick and mortar releases crystalline silica dust, which can cause serious lung disease. Cut wet whenever possible, using a wet saw or a grinder with water feed. Wear a properly fitted N95 or P100 respirator even when cutting outdoors, keep bystanders and pets away, and clean up with a HEPA vacuum or wet methods. Never dry sweep masonry dust.

Troubleshooting Brick Problems

White powder on the surface

That is efflorescence, salts carried out by moisture. Brush it off dry and fix the water source, such as poor drainage or missing caps.

Faces popping off (spalling)

Usually freeze-thaw damage from the wrong grade or water trapped by hard mortar or sealers. Replace damaged bricks with SW grade and improve drainage.

Patio bricks shifting or sinking

The base was too thin or poorly compacted. Lift the area, add and compact gravel, then reset.

General Cost Ranges

Common brick is the cheapest option, face brick costs more, and specialty colors, tumbled finishes and thin brick add further cost. Concrete brick usually undercuts clay. Installed brick walls and patios cost several times the price of the bricks themselves, because labor, base work and mortar make up most of the total.

When to Call a Pro

Low garden walls, borders and small sand-set patios are realistic DIY jobs. Hire a mason for retaining walls over about 3 feet, chimney repairs, load-bearing walls, structural cracks, or any wall near a property line that needs a permit. If you are matching red clay bricks on an older home, a mason can often source salvaged brick or blend new runs so repairs do not stand out.

Frequently Asked Questions

Why are clay bricks red?

Iron oxide in the clay turns red when fired in an oxygen-rich kiln. Clays with less iron fire to buff, cream or white.

What grade of brick should I use outdoors?

Use SW (severe weathering) grade for anything in contact with soil, laid flat, or exposed to freeze-thaw cycles. MW grade suits vertical walls in milder climates.

Can I use regular bricks for a patio?

Not cored building brick. Use solid paving brick rated for traffic and your climate, or water will collect in the holes and crack the brick.

Are clay bricks better than concrete bricks?

Clay holds its color longer and has a classic look, while concrete is often cheaper and more uniform. Both work when the grade matches the use.

How do I cut a red clay brick by hand?

Score all four faces with a brick chisel and hand sledge, then strike the scored line firmly. Wear eye protection and a respirator, and wet the brick to keep dust down.