A well-installed copper roof detail can outlast two or three asphalt roofs, which is the main reason people pay the premium. Copper flashing does not rust, holds solder joints for decades and weathers from bright penny to brown to the familiar blue-green patina without losing strength. It is the traditional choice for chimneys, valleys, bay window roofs and anywhere the flashing is visible enough that appearance matters.
Part of our Roofing guide — explore the full guide →
For most homes, 16 oz copper (sold by weight per square foot) is the standard for step flashing, counter flashing and drip edge. Heavier 20 oz copper is used for valleys, built-in gutters, long runs and high-wear spots. Copper works best when it is paired with copper gutters or a slate, tile or cedar roof that will last as long as the metal. On a 20-year shingle roof, copper is often more cosmetic than practical, because the flashing will be torn off and possibly reused long before it wears out.
Copper Flashing Weights, Forms and Uses
Copper sheet is described in ounces per square foot rather than gauge. A 16 oz sheet is roughly 0.0216 inches thick, and 20 oz is about 0.027 inches. Heavier copper is stiffer, resists denting and holds a crisp bend over long spans.
- Coil or roll stock: a copper flashing roll in widths from 6 to 24 inches lets you cut and bend custom pieces for aprons, valleys and counter flashing. It is the most flexible option for one-off details.
- Copper step flashing: pre-bent L pieces, usually 5 by 7 or 4 by 4 by 8 inches, for sidewalls where a roof meets a wall or chimney cheek.
- Copper counter flashing: stepped or straight pieces let into mortar joints on chimneys and masonry walls to cover the vertical legs of step flashing.
- Copper drip edge: preformed copper drip edge flashing in 10-foot lengths for eaves and rakes, often chosen to match copper gutters.
- Valley and pan flashing: wide 20 oz sheet, often with a center crimp to keep water from crossing the valley.
Copper roof flashing also comes in lead-coated and pre-patinated versions. Lead-coated copper starts gray and stays gray, while pre-patinated sheet arrives already green. Both cost more than bright copper.
Patina: What to Expect Over Time
Bright copper starts darkening within weeks. Over the first year or two it turns a uniform brown, then slowly darkens toward chocolate. The green patina (verdigris) usually takes 10 to 30 years to develop, depending on rain, humidity and air quality. Coastal and urban areas patina faster; dry inland climates may stay brown for decades.
Patina is a protective layer, not corrosion that weakens the metal. If you want to keep copper bright, you can apply a clear lacquer, but it requires reapplying and usually looks blotchy as it fails. Chemical patina solutions can speed up the green color, but results vary and they need careful handling.
One side effect matters on light-colored surfaces: rain running off copper carries traces of copper salts that leave green stains on stone, stucco, light siding and concrete. Plan drip edges and kickouts so runoff lands in gutters or on surfaces where staining is acceptable.
Tools and Materials
- Copper sheet, coil or pre-bent pieces in matching weight
- Copper or stainless steel nails and cleats (never galvanized or aluminum)
- Hand seamers, aviation snips and a sheet metal brake for long bends
- Soldering iron or torch, 50/50 or lead-free solder, and a flux made for copper
- Wire brush or abrasive pad for cleaning seams
- Self-adhered underlayment rated for high temperatures under soldered work
- Gloves with cut resistance and safety glasses
Installing Copper Flashing Step by Step
- Plan for movement. Copper expands and contracts noticeably with temperature. Hold long pieces with cleats rather than face nails, and use loose-lock or lap joints with sealant on runs longer than about 10 feet so the metal can move.
- Isolate dissimilar metals. Keep copper away from aluminum, galvanized steel and bare steel fasteners. Water that runs off copper onto aluminum gutters or galvanized flashing will eat through them. Use copper or stainless fasteners only.
- Underlayment first. Install high-temperature self-adhered underlayment at chimneys, valleys and walls, especially where you plan to solder.
- Base and step pieces. At a chimney or wall, install the front apron, then weave copper step flashing into each shingle or slate course, one nail high in the roof leg, never through the wall leg.
- Counter flashing. Cut reglets about 1 inch deep into mortar joints, bend a hem on the counter flashing for stiffness, insert, wedge with copper or lead wedges and point the joint with mortar or a compatible sealant.
- Solder the seams that need it. Clean both surfaces until bright, flux, tin the edges, then lap at least 1 inch and sweat solder through the seam. Soldered seams are used on chimney crickets, pans and corners where a lap alone cannot keep water out.
- Drip edge. Install copper drip edge under underlayment at eaves and over it at rakes, lapped 2 to 4 inches at joints and held with copper nails.
Soldering Safety and Ventilation
Soldering involves an open flame on a roof and heated flux that gives off fumes. Work with good airflow, keep your face out of the smoke, and wear gloves and eye protection. If you use leaded solder, wash your hands before eating and keep scraps away from children; lead-free solder is a better choice for most homeowners. Keep a fire extinguisher on the roof, let soldered areas cool before walking away, and check for smoldering underlayment or debris afterward. Clean flux residue with water so it does not keep reacting with the copper.
Ladder and Roof Safety
Copper sheet has sharp edges and long pieces catch wind, so carrying it up a ladder is risky. Hoist long stock with a rope instead of climbing with it. Set the ladder at a 4-to-1 angle, extend it 3 feet above the eave, tie it off and keep three points of contact. Use a roof harness anchored to framing on steep pitches, and never work on wet or frosty roofs. Chimney and valley work on two-story homes, slate or tile roofs belongs with a roofer or sheet metal contractor who has fall protection and scaffolding.
Troubleshooting Copper Details
- Green stains on siding or stone: redirect runoff with a kickout or extend the drip edge into the gutter.
- Cracked solder joints: usually caused by expansion on long runs with no movement joint. Add a loose-lock seam.
- Pinholes in aluminum gutters below copper: galvanic corrosion. Switch to copper gutters or redirect copper runoff away from them.
- Buckled valley: face nails pinned the metal; replace with cleated installation.
- Leaks at counter flashing: mortar or sealant in the reglet has failed. Clean out the joint and repoint.
Cost: What the Premium Buys
Copper costs several times more than aluminum or galvanized steel per square foot, and copper prices move with the metals market. Labor also runs higher because soldering and custom bending take skill. A copper chimney flashing package with step, counter and cricket can cost several times what an aluminum package does, often into the low thousands of dollars installed. Bulk copper roll stock is typically more economical than pre-bent pieces if you have a brake. The premium makes sense on long-life roofs (slate, tile, standing seam, cedar), historic homes and when you already have or plan copper gutters. On a standard shingle roof, aluminum or prefinished steel delivers the same water protection for less.
When to Call a Pro
Hire a roofer or sheet metal contractor for soldered work, chimney crickets, built-in gutters, slate or tile roofs and anything above the first story. A professional with copper experience will also detail expansion joints and metal separation correctly, the two issues behind most copper failures. Ask whether your local building department requires a permit for flashing replacement tied to a reroof.
Frequently Asked Questions
Is 16 oz or 20 oz copper better for flashing?
16 oz is standard for step, counter and drip edge on homes. 20 oz is better for valleys, built-in gutters, long runs and areas that take foot traffic or heavy water flow.
How long does copper flashing last?
Properly installed copper often lasts 60 to 100 years or more, which is why it is commonly reused or paired with long-life roofing materials.
Can copper flashing touch aluminum gutters?
No. Copper and aluminum react, and runoff from copper corrodes aluminum. Use copper gutters or keep the metals separated and redirect the water.
How long does it take copper to turn green?
Copper usually turns brown within a year or two. The green patina typically takes 10 to 30 years and develops faster in wet, coastal or urban air.
Do copper flashing seams need solder?
Simple laps work on step flashing and drip edge. Soldered seams are used on chimney crickets, pans, corners and built-in gutters where water would otherwise get through a lap.