Most cracks in brick walls are not a sign your house is falling down. Hairline cracks in mortar joints are common as masonry ages, shrinks, and moves with the seasons, and they are usually a routine brick crack repair job: rake out the damaged mortar and repoint the joint. Cracks that split through the bricks themselves, widen over time, or form a stair-step pattern wider than about 1/4 inch deserve closer attention because they can signal foundation settlement or wall movement.
The quick answer, then, depends on the pattern. Thin cracks confined to mortar joints are a DIY repair. A single cracked brick can be cut out and replaced in an afternoon. Wide, growing, or diagonal cracks, bulging walls, and cracks paired with sticking doors or sloping floors should be looked at by a structural engineer before you patch anything, because filling a moving crack only hides the evidence.
Below you will learn how to read what each crack means, the tools you need, step-by-step instructions for repointing and replacing a brick, troubleshooting tips, typical costs, and the red flags that call for a professional.
Brick Crack Repair Starts With Reading the Crack
Before you pick up a trowel, spend ten minutes studying the wall. The pattern, width, and location of cracks in brick mortar tell you whether you are dealing with cosmetic wear or active movement.
- Hairline cracks in mortar only: Usually shrinkage or weathering. Common and cosmetic.
- Stair-step cracks through mortar joints: Often caused by differential settlement. Under 1/8 inch and stable is usually minor; over 1/4 inch or growing warrants an engineer.
- Vertical cracks: Can come from thermal expansion on long walls without expansion joints, or from settlement at one end. Cracks wider at the top than the bottom suggest a corner is dropping.
- Horizontal cracks: In a brick veneer, may point to rusted steel lintels or wall ties. In a foundation or solid masonry wall, horizontal cracking can indicate lateral pressure and is a structural concern.
- Cracks through the brick faces: Point to significant stress, freeze-thaw damage, or brick that is softer than the mortar around it.
- Cracks above windows and doors: Frequently caused by a rusting, expanding lintel. The steel needs attention, not just the mortar.
Monitor Before You Repair
If you are unsure whether cracks in brick house walls are still moving, monitor them for a few months. Mark each end of the crack with a pencil line and the date, measure the width with a crack gauge or feeler gauge, and photograph it next to a ruler. Check again after heavy rain, a dry spell, and a freeze. A crack that stays the same width is usually safe to repair cosmetically. A crack that grows, lengthens past your marks, or opens and closes seasonally by more than a hairline should be evaluated by a professional.
Tools and Materials
- Safety glasses, work gloves, and an N95 or better respirator (cutting mortar and brick creates crystalline silica dust)
- Angle grinder with a diamond tuck-point blade, or a plugging chisel and 2-lb hand sledge
- Joint raker, tuck-point trowel, and brick trowel
- Mortar hawk or scrap plywood board
- Jointing tool that matches your existing joint profile (concave, V, or flush)
- Pre-mixed Type N or Type O mortar for most older brick; Type S only where specified
- Replacement bricks matched in size, color, and hardness (salvage yards are a good source)
- Spray bottle, stiff nylon brush, and bucket
Mortar choice matters more than most people think. Mortar should be softer than the brick so the joint, not the brick, absorbs movement. Using a hard, high-cement mortar on old soft brick is a leading cause of spalled brick faces. For homes built before about 1930, a lime-based mortar is often the right match; a masonry supplier can help.
How to Repoint Cracked Mortar Joints
Repointing, also called tuck-pointing, is the most common fix for cracks in brick mortar and the backbone of most cracked brickwork repair.
- Protect yourself and the area. Wear eye protection and a respirator, and lay a tarp below the wall. Work in temperatures between roughly 40°F and 90°F.
- Remove damaged mortar. Rake or grind out cracked mortar to a depth of about 2 to 2.5 times the joint width, typically 1/2 to 3/4 inch. Keep the grinder blade centered in the joint so you do not chip brick edges.
- Clean the joints. Brush out dust and loose particles, then mist the joints with water. Damp masonry keeps the new mortar from drying too fast.
- Mix the mortar. Add water gradually until the mortar has the consistency of stiff peanut butter. Let it slake for 5 to 10 minutes and remix.
- Fill in layers. Press mortar into the joints with a tuck-point trowel, filling deep joints in 1/4-inch layers and letting each firm up to thumbprint hardness before adding the next. Fill head (vertical) joints before bed (horizontal) joints.
- Tool the joints. When the mortar is firm but still takes a thumbprint, strike it with a jointing tool to match the existing profile. Tooling compresses the mortar and sheds water.
- Clean and cure. Brush off crumbs once the mortar is stiff. Mist the repair lightly two or three times a day for three days to help it cure, and keep it out of direct hot sun if possible.
How to Fix Cracked Brick by Replacing It
When a crack runs through the brick itself, patching the face rarely lasts. Replacing the unit is the better way to fix cracked brick, as long as the underlying movement has stopped.
- Grind or chisel out the mortar around all four sides of the damaged brick.
- Break the brick into pieces with a plugging chisel, working from the center outward, and remove the fragments. On a veneer wall, avoid damaging the wall ties behind it.
- Clean all old mortar from the cavity and dampen the surrounding brick.
- Butter the bottom and sides of the opening and the top and ends of the new brick with mortar.
- Slide the brick into place, tapping it flush with the trowel handle. Pack any gaps with extra mortar.
- Tool the joints to match and mist to cure over the next few days.
Troubleshooting Fixing Cracked Brickwork
- New mortar is the wrong color. Mortar dries lighter. Make test batches with colored pigment, let them cure on a scrap board for a week, and compare in daylight.
- Crack reappears in the same spot. The wall is still moving. Stop patching and have the cause assessed.
- Brick faces flaking after repair. The mortar is harder than the brick or water is trapped behind the wall. Switch to a softer mortar and check gutters and grading.
- White haze on the wall. That is efflorescence from salts carried by moisture. Brush it off dry and fix the water source.
- Mortar crumbling within weeks. It dried too fast or froze. Keep it damp and do not repoint when frost is forecast within 48 hours.
Typical Costs
DIY repointing materials are inexpensive: a bag of pre-mixed mortar is usually $10 to $25, and a diamond tuck-point blade runs about $25 to $60. Professional repointing is commonly priced per square foot and varies with access, mortar type, and region, often falling in the range of several dollars to $20 or more per square foot. Replacing a handful of cracked bricks might cost a few hundred dollars from a mason, while lintel replacement or rebuilding a section of wall costs considerably more. A structural engineer’s evaluation typically runs a few hundred dollars and is money well spent if you see red-flag cracking.
When to Call a Structural Engineer
Brick walls carry real loads, and some cracks are symptoms of problems below or behind them. Get a structural engineer or experienced foundation contractor involved before any brick crack repair if you notice:
- Stair-step or vertical cracks wider than about 1/4 inch, or any crack that is getting wider
- Horizontal cracks in a foundation wall or load-bearing masonry
- Bulging, leaning, or bowing brick sections, or brick separating from window and door frames
- Doors and windows that suddenly stick, sloping floors, or new drywall cracks inside
- Cracks above openings with visible rust or a sagging lintel
- Chimney cracks, leaning chimneys, or loose bricks near the roofline
An engineer can tell you whether the cause is soil settlement, poor drainage, tree roots, failed wall ties, or lintel corrosion, and specify the right repair. A licensed mason then handles the masonry work, and a foundation contractor handles underpinning or other structural fixes. Patching first and investigating later only makes the diagnosis harder.
Frequently Asked Questions
Are cracks in brick mortar normal?
Hairline cracks in mortar joints are common as masonry ages and weathers. They are usually cosmetic, but repointing them keeps water out and prevents freeze-thaw damage from spreading.
When should I worry about cracks in my brick house?
Worry when cracks are wider than about 1/4 inch, keep growing, run horizontally in a foundation, or come with sticking doors, sloping floors, or bulging walls. Have a structural engineer evaluate those.
Can I use caulk for brick crack repair?
Caulk is a stopgap at best. It does not match mortar, traps moisture, and hides movement. Repointing with the correct mortar type is the proper repair for masonry joints.
What mortar should I use for cracked brickwork repair?
Most residential brick uses Type N mortar, and older soft brick often needs Type O or a lime mortar. The mortar should always be softer than the brick around it.
How long does repointed mortar take to cure?
Mortar is firm within a day, but it keeps curing for weeks. Mist it for the first three days and protect it from freezing temperatures for at least 48 hours.